摘  要: 考察了贫化温度、硫化剂、还原剂、缓冷速率等因素对炼铜水淬渣中铜回收指标的影响。试验表明,当贫化温度保持在1350℃、硫化剂黄铁矿配比为5%、还原剂煤粉与硫化剂之比为1∶4、缓冷速率为5K/m in时,可获得粗选铜回收率78%左右、粗选精矿铜品位5.8%左右的技术指标。 The factors influencing copper recovery, such as impoverishment temperature, curing ingredient, reductant and the velocity of slow cooling were studied. The results indicated that the optimal impoverishment-flotation efficiency was obtained when the impoverishment temperature is kept at 1350℃,the dosage of the iron pyrite is 5%,the mixture ratio of the reductant coal fines and curing ingredient is 1 : 4, and the velocity of slow cooling is 5K/min. A concentrate of 5.8% copper content and a copper recovery of 78% is produced.

关 键 词: 水淬渣 贫化 浮选

领  域: [环境科学与工程]

相关作者

相关机构对象

相关领域作者

作者 覃剑
作者 王逢文
作者 崔书琴
作者 吴贤静
作者 吴大磊