机构地区: 暨南大学生命科学技术学院化学系
出 处: 《化学研究与应用》 2006年第2期204-206,共3页
摘 要: We have successfully synthesized carbon nanotubes by the solvothermal approach at 400℃,in which toluene was used as the carbon source and solvent,and LaNi5 was used as the catalyst.The products were characterized with X-ray powder diffractometer(XRD),transmission eletronic microscopy(TEM)and Raman spectroscopy.The results show that the products are hexaganol phase carbon nanotubes with inner diameters ranging from 5 to 10nm and outer diameters approximately 100nm.The length of the carbon nanotube is of several micrometres. We have successfully synthesized carbon nanotubes by the solvothermal approach at 400℃, in which toluene was used as the carbon source and solvent, and LaNi5 was used as the catalyst. The products were characterized with X - ray powder diffractometer(XRD) ,transmission eletronie microscopy(TEM)and Ramnn spectroscopy. The results show that the products are hexagand phase carbon nanotubos with inner diameters ranging from 5 to 10nm and outer diameters approximately 100nm. The length of the carbon nanotube is of several micrometres.
领 域: [一般工业技术]